Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 5.86 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 5.86 MPa
850 psi
Stabilized, typ
Hexcel® HexWeb® HRH-10/F50 - 5.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglass cloth reinforc..
Compressive Yield Strength >= 5.86 MPa
>= 850 psi
Bare, min
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Yield Strength >= 5.86 MPa
>= 850 psi
Bare, min
Hexcel® HexWeb® HRH-10 - 1/8- 6.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 5.86 MPa
850 psi
Aptek DI-STRATE 1500-1 Microwave/RF Foam Substrate
DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Iridium Satellite AntennasInformation provi..
Copyright © lookpolymers.com All Rights Reserved