Polymer Property : Compressive Yield Strength = 522 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 3.60 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
522 psi

@Strain 1.00 %,
Time 1000 hour
ASTM D695
Manifattura Cattaneo RULON® J Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Compressive Yield Strength 3.60 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
522 psi

@Strain 1.00 %,
Time 1000 hour
ASTM D695
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Copyright © lookpolymers.com All Rights Reserved