Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 370 MPa | 53700 psi | ISO 14126 |
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Compressive Yield Strength | 370 MPa @Temperature 150 °C |
53700 psi @Temperature 302 °F |
90º, Wet; EN2850 Type B |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |