Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 3.90 MPa | 565 psi | Bare, typ |
Hexcel® HexWeb® HRH-10/F50 - 4.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |