Polymer Property : Compressive Yield Strength = 59500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 156 - 410 MPa
22600 - 59500 psi
Average value: 250 MPa Grade Count:23
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..