Mechanical Properties Metric English Comments
Compressive Yield Strength 480 MPa
69600 psi
ASTM E8
3D Systems LaserFormâ„¢ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing
Parts fabricated from this rapid prototype metal material are actually a blend of stainless steel and bronze. The part is built with steel and subsequently infiltrated with bronze. A6 is great for ..