Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 7.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 7.00 MPa
1020 psi
Typical; ASTM C365
Parabeam Industrie ParaTank 4.5 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Compressive Yield Strength 7.00 - 23.4 MPa
1020 - 3400 psi
Average value: 11.7 MPa Grade Count:7
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min..
Compressive Yield Strength 7.00 - 100 MPa
1020 - 14500 psi
Average value: 46.3 MPa Grade Count:6
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon
PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard ..
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Compressive Yield Strength 7.00 - 11.0 MPa

@Strain 1.00 %
1020 - 1600 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Copyright © lookpolymers.com All Rights Reserved