Polymer Property : Compressive Yield Strength = 7.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 6.50 - 7.50 MPa

@Strain 1.00 %
943 - 1090 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite
PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss..