Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 7.80 MPa | >= 1130 psi | ASTM C365 |
Parabeam Industrie Paraglass 3 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Compressive Yield Strength | 7.80 MPa | 1130 psi | ASTM D695 |
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |