Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 745 MPa | >= 108000 psi | |
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |