Compressive Yield Strength >= 5.40 MPa
>= 783 psi
ASTM C365
Parabeam Industrie ParaTank 4.5 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Compressive Yield Strength 5.40 MPa
783 psi
Sawbones Second-Generation Simulated Cancellous Bone (Cellular)
Rigid Polyurethane BoneSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous ma..
Compressive Yield Strength 5.40 MPa
783 psi
Sawbones Third-Generation Simulated Cancellous Bone (Cellular)
Rigid Polyurethane BoneSawbones® standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid..
Compressive Yield Strength 5.40 MPa
783 psi
Sawbones Cellular Rigid Polyurethane Foam 20 pcf Density
Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone ..