Polymer Property : Compressive Yield Strength = 8160 psi
Polymer Property :
Compressive Yield Strength =
8160 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Yield Strength
56.3
MPa
8160
psi
ASTM D695
Devcon Carbide Putty Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.