Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.570 MPa | 82.7 psi | Compressive Load Deflection at 15%; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2550 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Compressive Yield Strength | 0.570 MPa | 82.7 psi | Compressive Load Deflection at 20%; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |