Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 852 MPa | 124000 psi | EN2850B |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel |