Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.90 - 6.20 MPa @Strain 1.00 %, Time 3.60e+6 sec |
856 - 899 psi @Strain 1.00 %, Time 1000 hour |
ASTM D695 |
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |