Mechanical Properties Metric English Comments
Compressive Yield Strength 87.49 MPa
12690 psi
Abatron AboCast 50-16/AboCure 50-12 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours..