Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0650 MPa | 9.43 psi | TSM 1501 G 2A4 |
Eurofoam Porocell POR 302/T NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |
|||
Compressive Yield Strength | 0.0650 MPa @Strain 25.0 % |
9.43 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 302/T NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |
|||
Compressive Yield Strength | 0.0650 - 0.0900 MPa | 9.43 - 13.1 psi | 25% Compression |
BIW ASTM Class 2D3 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |