Polymer Property : Compressive Yield Strength = 9.70 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 9.70 MPa
1410 psi
at 10% deflection, parallel to thickness
Zircar Refractory Composites RS-A2 Refractory Sheet
This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee..