Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 9.9974 - 6500 MPa @Temperature 60.0 - 177 °C |
1450.0 - 943000 psi @Temperature 140 - 351 °F |
Average value: 1030 MPa Grade Count:6 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |