Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 634 MPa | 92000 psi | |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |