Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.50 - 6.50 MPa @Strain 1.00 % |
798 - 943 psi @Strain 1.00 % |
ASTM D695 |
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne.. |