Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 97.9 MPa | 14200 psi | ASTM D695 |
Diapolyacrylate Acrypet® MF-001 PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |