Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 10.0 kN/m @Temperature 100 °C |
57.1 pli @Temperature 212 °F |
TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 181-64 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Graves Tear Strength | 10.0 kN/m @Temperature 100 °C |
57.1 pli @Temperature 212 °F |
TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |