Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00580 GPa | 0.841 ksi | at 15% Compression; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2750 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |