Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0000500 GPa | 0.00725 ksi | at 20% compression; ISO 7743 |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |