Compressive Modulus 0.00240 - 0.0392 GPa
0.348 - 5.69 ksi
Average value: 0.0153 GPa Grade Count:29
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..