Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0896 - 0.124 GPa | 13.0 - 18.0 ksi | TM R050-38 |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Compressive Modulus | 0.0896 GPa | 13.0 ksi | Stabilized, typ |
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Compressive Modulus | 0.0896 - 0.124 GPa | 13.0 - 18.0 ksi | TM R050-38 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |