Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Modulus = 0.117 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.117 GPa
17.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 3/8 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Modulus 0.117 GPa
17.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10/OX - 1/4 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Modulus 0.117 GPa
17.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10/OX - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Copyright © lookpolymers.com All Rights Reserved