Polymer Property : Compressive Modulus = 0.138 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.138 - 4.14 GPa
20.0 - 600 ksi
Average value: 2.97 GPa Grade Count:9
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Compressive Modulus 0.138 GPa
20.0 ksi
Stabilized, typ
Hexcel® HexWeb® CR III 3/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Modulus 0.138 GPa
20.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Modulus 0.138 GPa
20.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Modulus 0.138 GPa
20.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Modulus 0.138 GPa
20.0 ksi
Stabilized, typ
Hexcel® HexWeb® CR III 1/4-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Modulus 0.138 GPa
20.0 ksi
Stabilized, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..