Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.160 GPa | 23.2 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic.. |