Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | >= 0.240 GPa | >= 34.8 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Compressive Modulus | 0.240 GPa | 34.8 ksi | |
Hexcel® HexWeb® CRF-3/8-ACG-.002-2.3 Chromate free ACG® Honeycomb Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app.. |