Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Compressive Modulus 0.430 GPa
62.4 ksi
ASTM D695
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.