Mechanical Properties Metric English Comments
Compressive Modulus 0.448 GPa
65.0 ksi
ASTM D695
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
Compressive Modulus >= 0.448 GPa
>= 65.0 ksi
Engineered Syntactic Systems SF-22 Subsea Macrosphere Syntactic Void Filler
In applications where density is critical, the four part SF-22 kit is used. This system utilizes fiber reinforced epoxy macrospheres in combination with the standard microsphere syntactic to provide..
Compressive Modulus 0.448 GPa
65.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRP - 3/8 - 4.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Modulus 0.448 GPa
65.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRP/OX - 1/4 - 5.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Modulus 0.448 GPa
65.0 ksi
TM R050-38
Resinlab® SEC1222 Silver Filled Epoxy Adhesive
Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit..