Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet)
|
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet)
|
Compressive Modulus |
0.552 GPa @Temperature 22.8 °C
|
80.0 ksi @Temperature 73.0 °F
|
ASTM D695 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE
|
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
|
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f.. |
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
|
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet)
|
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP Tivar® Premium UHMW-PE Tivar Premium UHMW-PE
|
Compressive Modulus |
0.552 GPa |
80.0 ksi |
Stabilized, typ, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 1/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
Compressive Modulus |
0.552 GPa |
80.0 ksi |
ASTM D695 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet)
|