Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.558 GPa | 80.9 ksi | ASTM D695 |
Saint-Gobain Fluoroloy® A01 High Performance Seal Material Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved.
Information provide.. |