Compressive Modulus 0.579 GPa
84.0 ksi
ASTM D695
Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet)
Compressive Modulus 0.579 GPa
84.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRP - 1/4 - 5.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Modulus 0.579 GPa
84.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..