Compressive Modulus 0.648 GPa
94.0 ksi
ASTM D695
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet)
Compressive Modulus 0.648 GPa
94.0 ksi
ASTM D695
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet)