Polymer Property : Compressive Modulus = 0.958 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.958 GPa
139 ksi
ASTM D695
Greene Tweed ARâ„¢ 1 Abrasive-Resistant Thermoplastic
Sand and other abrasives are often a challenge for pump users in the power industry. Clearances on line shaft bearings and bowl wear rings open up, increasing pump vibrations and reducing pump effi..