Polymer Property : Compressive Modulus = 1.035 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.035 GPa
150.1 ksi
Z direction; ASTM D638
Rogers Corporation RT/duroid® 6202 High Frequency Laminate
Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric..
Compressive Modulus 1.035 GPa
150.1 ksi
Z direction; ASTM D638
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate
Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric..