Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00220 - 0.00760 GPa | 0.319 - 1.10 ksi | Average value: 0.00416 GPa Grade Count:10 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |