Polymer Property : Compressive Modulus = 1.55 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0107 GPa
1.55 ksi
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..
Copyright © lookpolymers.com All Rights Reserved