Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.71 GPa | 248 ksi | cured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C, 13 mm/min; ASTM D695-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |