Mechanical Properties Metric English Comments
Compressive Modulus >= 0.0750 GPa
>= 10.9 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..