Polymer Property : Compressive Modulus = 102 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.600 - 0.700 GPa

@Strain 0.200 %
87.0 - 102 ksi

@Strain 0.200 %
ASTM D621
Dalau Dalcon 001 100% Virgin PTFE
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi..
Compressive Modulus 0.600 - 0.700 GPa

@Strain 0.200 %
87.0 - 102 ksi

@Strain 0.200 %
ASTM D621
Dalau Dalcon 001 100% Virgin PTFE
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi..