Polymer Property : Compressive Modulus = 11.6 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus >= 0.0800 GPa
>= 11.6 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T90.150 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Compressive Modulus >= 0.0800 GPa
>= 11.6 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Compressive Modulus >= 0.0800 GPa
>= 11.6 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..