Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.758 GPa | 110 ksi | ASTM D695 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Compressive Modulus | 0.758 GPa | 110 ksi | ASTM D695 |
Saint-Gobain Fluoroloy® A16 High Performance Seal Material General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service
Information provided by Saint-Goba.. |
|||
Compressive Modulus | 0.759 GPa | 110 ksi | |
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Compressive Modulus | 0.758 GPa | 110 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 5/32-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 0.758 GPa | 110 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |