Polymer Property : Compressive Modulus = 1150 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 7.93 GPa
1150 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil..
Compressive Modulus 7.93 GPa
1150 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber
Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s..