Mechanical Properties Metric English Comments
Compressive Modulus 12.0 - 162.027 GPa

@Temperature -55.0 - 177 °C
1740 - 23500.4 ksi

@Temperature -67.0 - 351 °F
Average value: 62.1 GPa Grade Count:16
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Compressive Modulus 12.0 GPa

@Temperature 100 °C
1740 ksi

@Temperature 212 °F
90º, Wet; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel