Polymer Property : Compressive Modulus = 12.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0830 GPa
12.0 ksi
average; perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to ..