Polymer Property : Compressive Modulus = 1240 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 8.55 GPa
1240 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
Compressive Modulus 8.55 GPa
1240 ksi
ASTM D695
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..